Product​


pRODUCT

-------------

A182 F51,S31803,2205,1.4462 plate,strip,wire rods,bar,wires
    发布时间: 2020-04-11 15:27    
A182 F51,S31803,2205,1.4462 plate,strip,wire rods,bar,wires

S31803 /2205 /F51/1.4462 Super Duplex stainless steel

Name

OD
(mm)

Thickness
(mm)

Length
(m)

Seamless tube

Φ6~630

1~50

specified or non-specified

Round bar

Φ8~250

 

specified or non-specified

Fastener

M8~M200

 

 

S31803 /2205 /F51/1.4462 Super Duplex stainless steel Chemical Composition

Grade

C

Mn

Si≤

S

P

Cr

Ni

Mo

N

PREN

S31803(2205)
022Cr19Ni5Mo3Si2N

0.03

2.0

1.0

0.02

0.03

21-23

4.5-6.5

2.5-3.5

0.08-0.2

 

35

S31803 /2205 /F51/1.4462 Super Duplex stainless steel Mechanical Properties

Grade

 

Heat treatment

 

Tesile Strength
Rm(Mpa)

 

Yield Strength
Rp(Mpa)

 

A%

 

Reduction
%
Min

 

Hardness

Brinell
HB

S31803(2205)F51
022Cr19Ni5Mo3Si2N

1020
Water quenching

620

450

25

 

45

 

≤293

S31803 Producing Standard

Specification

Seamless and welded tube

Bar

Sheet/strip

Forging
(Flange)

Casting

S31803(2205)F51
022Cr19Ni5Mo3Si2N

ASTM A789
ASTM A790
ASTM A1016
ASTM A999
ASTM A928

ASTM A276
ASTM A479
ASTM A76

ASTM A240

ASTM A473
ASTM A182

ASTM A351
ASTM A995

31803 Properties Introduction

Duplex 31803 is a two-phase, ferritic, austenitic 22% chromium, 3% molybdenum, 5 to 6% nickel alloyed stainless steel. It is the most widely used duplex stainless steel grade and is characterized by high yield strength, double that of the standard austenitic stainless steel grades. It also demonstrates good fatigue strength, as well as outstanding resistance to stress corrosion cracking, crevice, pitting, erosion, and general corrosion in severe environments.

The following are the properties of 31803:

Stainless ferritic-austenitic Cr-Ni-Mo steel with nitrogen addition.
High corrosion resistance, especially against stress corrosion cracking in solutions containing chloride.
Good strength properties.
Resistant to intergranular corrosion in the temperature range up to 300°C.
Heat treatment subsequent to welding not necessary.
Surface condition for optimum corrosion resistance: pickled, heat treated free from scale or machined.